Can stellite 6 be welded to inconel 800H? I have been told that it can be welded with inco82 consumable but dont have the ability to do a lot of trial and error for procedures if it cant,...anybody got any info? will the stellite crack?...Alex
I have to admit I haven't tried it, but I expect it would crack. Stellite 6 is prone to cracking anyway, even when you're welding on top of it with Stellite 6. If you HAD to weld it to 800H, you would probably have to use Stellite 6 rod.