Hello all,
I agree with jon on the maximum gap being flexible.
We have minimum gaps allowable which I have always thought was to counter any weld shrinkage/stress problems.
The socket weld is going to be a fillet weld so as long as the gap is greater than the minimum required you are safe.
Off the top of my head I am not 100% sure that B31.3 doesn't give maximums and minimums.
Looks like I am jumping in the codes first thing in the morning
Regards,
Shane
By anuss
Date 11-15-2006 14:34
I have, in the past, gone with thickness being the max allowed gap, guess I would like to be assured on this one. :-)
Thanks!
Agreed, B31.3 states the minimum welding dimensions in para. 328.5.2 and fig. 328.5.2.c but no max. dimensions for gap are given.
Interpretation: 6-02
Subject : ANSI/ASME 83 1.3-1 984 Edition, with the ANSi/ASME B31.3a-1984 Addenda,
Para. 31 1.2.4 and Figs. 327.4.28 and C; Socket Welds, Gap Dimension
Date issued: December 14, 1987
File: 83 1-87-01 3
Question (1): In ANSI/ASME B31.3, para. 311.2.4(b)(2) states, "Weld dimensions shall not be less
than those shown in Figs. 327.4.2B and C." In Figs. 327.4.2B and C, there is a dimension that reads
"'1/16 in. approx. before welding." Do the above words mean that the gap should be no larger than
1/16 in.?
Reply (1 ): No.
Question (2): If the response to Question (1) is no, how large a gap would be acceptable?
Reply (2): The '''1/16 in." is not a "welding dimension." It is intended as an "approximate"
dimension for nominal clearance.
(Edited to add Interpretation)
I am sure ASME has reasons for not being too prescriptive over the min and maximum gap sizes, before and after welding however to control this from a QC/NDT point of view becomes difficult when the approximate gap of 1.5mm is stipulated before welding. This leaves room for the contractor /fabricator to argue the point that there was a 1.5mm gap before welding but has now closed due to welding shrinkage. This cannot be proven via the only practical method ie. RT.
I believe an after welding gap should be stipulated as minimum 1mm. All the fitter needs to do is push the pipe in all the way to the socket shoulder, scribe the pipe, withdraw it 2mm (or an amount this contractor has proved sufficient for that pipe size/welding procedure), tack and weld. Any deviation to the requirement of 1mm gap is cause for rejection - simple.
Residual weld stresses in a socket joint through no gap are an uneccessary evil, when added to other forces like internal pressure, misalignment of piping, vibration, impacts and other unforseen loadings can and have resulted in failures.
SA Inspector,
When I worked for SGS in New Zealand as a Radiographer we were regularly hired by the major oil companies to radiograph socket joints to prove that there was a gap.This was not a code requirement but a customer requirement (I presume to keep the contractor "on his toes")
Regards,
Shane
Hello everyone, I know I'm coming into this late but G.A.L does offer a water salable Gap-O-Let. The only Problem is G.A.L cannot give you a detail sheet to find out what's in it. The job I'm on has a halogen and chloride stipulation in the contract so we can't use them because we can't be sure what's in the material that the Gap-O-Let is made out of.
Thanks
Jim Hughes