hogan, thanks,
So by taking Table 2.3 into account, I can use E70 series wire on all these connections because it matches the base metal for some splices, but more importantly, because of 2.3 I am allowed to use a "filler metal with a strength level one classification less than matching".
Thanks for your input, Chris