Doe's anyone know if 7028 is still being produced in the U.S.? I've looked at Lincoln and Hobart websites, it seems to have been dropped those folks. Any help would be great.
John, Thanks for the infomation. I guess it's going back to 3/16" 7018 for the time being. Boy I really don't what to tell the shop about this little item.
our lincoln rep told us they pulled E-7028 because someone used it for "an applcation other than its intended purpose" and then lincoln got in trouble. sounded like a bunch of crap to me.