John,
Immediate repair and ship to a zinc mine in upstate New York. We put two shifts in over the weekend and plan on shipping back to the mine next Sunday. There is also extensive cracking in other loactions that is being repaired. Maintaining pin hole alignment is going to be our next concern, but I'm confident that the customer and the welding contractor will do a top notch job.