- - By 2003440 (**) Date 02-24-2007 00:22
need parts for a sa200 f163
Parent - - By raftergwelding (*****) Date 02-24-2007 12:05
what do you need i have a machine i'm parting out
Parent - - By 2003440 (**) Date 02-24-2007 18:00
Hello i need some side doors in great shape for a code 7693 sa200 it is a f163 machine.i think it is a 1976.
Parent - By raftergwelding (*****) Date 02-25-2007 01:34
only doors i have are warped from heat they may or maynot be able to straiten if ur intrested i'll sell the set for 100 plus freight