![](/mwf/attachments//avatars/13260-9338.jpg)
Ok i'm trying to see if i have to write a new WPS and qualify a new procedure. I'm looking up under prequalified base materials and fillers (table 3.1) to see what i have to work with. The materials we're welding on are below , Fillers are metalloy (80 d2 AWS A5.28 ASME SFA 5.28 E90C-D2) and for solid wire (AWS A 5.28 ASME SFA-5.28 ER80S-D2)
A36 not preq because of filler wire we're using
A441 not preq because of filler wire we're using
A656 not preq becuase it's not on the list
HI form 50 A715 not preq , not on list
A572 grade 50 not preq, not on list
A514 t-1 not preq, not on list
So i'm thinking i have to go and write a new WPS for each base matl with each filler rod and qaulify a new procedure for each. Can someone tell me if i'm doing this right?