I have a 67 model sa 200 that has been sitting for a while. It runs good but will not idle up when an you strike an arc. It has the pc board on it. When i put the machine on high idle, it will idle up and weld, but it is arcing out real bad between the armature and brushes. I notice that the steel band that the brushes sit in have rusted and will not let the brushes float. I have tried to free them by very lightly taping on them but have had no luck. What is the best way to get them to glide freely without tearing anything up? Is this why it wont idle up automatically? I did use a stone to clean the armature and exciter.
Thanks
Trey