This is one of those subjective questions...read D1.1:2006 Paragraph 5.15
--- this part of this paragraph is what trips us up with welding on galvanized....
" Surfaces on which weld metal is to be desposited shall be......<snip>........
Surfaces to be welded, and surfaces adjacent to the weld, shall also be free from ....<snip>....
other foreign material that would prevent proper welding or produce objectionable fumes."
Obviously galanizing is foreign material that would prevent proper welding, and it also produces objectionable fumes, so I think they spelled out galvanizing without actually coming out and naming it perse'.