SubArc is Simi-automatic (like GMAW and FCAW) and qualification is the same as with all Processes.
Just because a person is qualified for a manual process such as SMAW or GTAW does not qualify them for SAW or any other process other than the ones they are qualified in.
There are other Esential Variables that discribe the ranges of qualifaction in a process.