ok the saddle part is no problem, but do they want kind of bevel and are they looking for 100% penitration. the p5 down hill is no problem I am just trying to get as much info as I can. This will be the first time I will have taken this test and I want to get it right the first time.
It's the two references you've mentioned that I refer to. Usually, the standard Section IX rules apply except in those incidences.
328.2.2 Procedure Qualification by Others. Each
employer is responsible for qualifying any welding procedure
that personnel of the organization will use. Subject
to the specific approval of the Inspector, welding
procedures qualified by others may be used, provided
that the following conditions are met. (a) through (i)
(i) The employer has at least one currently employed
welder or welding operator who, while in his employ,
has satisfactorily passed a performance qualification test
using the procedure and the P-Number material specified
in the WPS. The performance bend test required
by Section IX, QW-302 shall be used for this purpose.
Qualification by radiography is not acceptable.
In this incidence, it's in relation to a PQR by others, but can apply
depending on conditions.
K328.2.1 you've already mentioned.
Therefore If a B31.3 test is specified, it's one of the two with the K328 being the most likely, otherwise a section IX test is specified and applied.
The question put forth stated a b31.3 test. Not a section IX test, and therefore is either confused or specifically refering to one of these two scenerios.
Regards,