![](/mwf/attachments//avatars/13260-9338.jpg)
I could of sworn i saw something about your backing material had to be the same material as that of your strongest plate for qualifying a WPS or for whatever application. I looked all over under backing and now i can't find it and i was wondering if someone could help. Example I'm quailfying a piece of A514 to a piece of A572 does the backing bar have to be A514 T-1 One more thing that maybe you guys can help me out on P.123 of d1.1 2006 4.7.3 base metal qualification it says steels listed in table 4.9 (A514)being one shal also qualify table 3.1 or table 4.9 steels in conformance to table 4.8. I'm haveing probs interpriting table 4.8 and was wondering if i qualify a test plate of 2 A514's does that save me from haveing to qualify table 3.1 steels with the same filler and from haveing to do any more procedures of table 3.1 steels to A514?
One more thing i promise!!! Does it say anywhere that you have to use the same tensile filler as the base metal you are welding on or is that just recomended.? We're using and 80 and 90psi wire on A514 t-1 that has a 100 to 130 ksi tensile range and i found that kind of od. Do you guys think the tensile pulls will come out using an 80psi wire?