![](/mwf/attachments//avatars/13260-9338.jpg)
Ok i have a crack in a shear point on one side of a truck frame channel. I don't know the ASTM # on the steel but i do have all the goodies so lets see what you guys think it is and how to repair.
It's a heat treated steel
Yield ksi min = 120
Ultimate Tensile ksi min = 125
% elongation in 2" 12
Brinell hardness 269-331
Here's my delima do i match the tensile to a matching filler or do i repair with something thats going to give alittle bit with a lesser tensile. I'm going with GTAW process with a full penn weld from one side. It's in a tight spot so i'm gona drill a hole where the crack stops and bevel it with single U groove with a dremel. Going to keep an eye on interpass temps also. So what do you guys think?
Thanks Kix..