OUR SHOP IS LOOKING INTO AISC CERTIFICATION, BUT REGARDLESS OF THAT, INSTILLING A TRUE QUALITY PROGRAM. I HAVE BEEN ELECTED TO DO THIS. ONE OF MY HURDLES IS IN TRYING TO DO THIS ALONE, HOW TO INSPECT 100% DIMENSIONS, AND ALSO 100% OF WELDS IN TRYING TO KEEP UP WITH A DOZEN WELDERS AND A BEAMLINE. I AM LOOKING TO GET MY CWI'S AND CAN CONFIDENTLY CHECK THE WELDS MYSELF AS THIS IS ALL I HAVE DID FOR TWENTY YEARS IN TAKING WELDING , TEACHING WELDING, AND BEING ON THE FLOOR AND MANAGEMENT. IF I USE THE GUYS ON THE FLOOR TO CHECK WELDS, WHAT KIND OF TRAINING WOULD BE BEST TO DOCUMENT THEY ARE CAPABLE OF VISUAL EXAMINATION FOR SOMEONE LIKE AN AISC AUDITOR. ANYBODY ELSE IN THIS SPOT OR BEEN IN IT? ALL HELP WOULD BE GREATLY APPRECIATED. THANKS