Mild steel/cold rolled steel: Mild steel is a term refering to steel with a low carbon and insignificant alloy percentages, while cold rolled steel refers to the finish rolling of the material being done cold rather than at red heat. Cold rolled steels could have up to about 40 point carbon, altho most are much lower, generally 5 point to 20 point.