We have a small machine, basically a tig welder in a box, the crossed ends of the two wires is clamped very closely with copper jaws, the joint is positioned under a tungsten electrode, argon gas is used, the arc is struck for an instant, and a welded ball is formed joining the two wires. You can work out a way to do this by hand on the bench.
How do you leak check wire?