Hi Gang!
I have been approached from a friend, to tig weld a few pieces of stainless steel door trim off a 55 Chevy. Two pieces are about to rub through, just need to be built up, filed, sanded and buffed. The other two pieces have about a 1/4" to 3/8" long cracks to be repair on the ends.
Any suggestions on what parameters to start with; I have a Dynasty 200 with a #9 torch, glass lenses and tunstens down to .020", and straight argon. Do I need to back purge with argon?
What filler rod should I use, THE TRIM PIECES ARE MAGNETIC. These are on a restoration project and I have been supplied with similar (garbage trim which I requested) to practice on.
Thanks,
NDAV8R