Hows everybody doing. I was wondering if anybody was familar with the lincoln ranger 305 and what they thought about compared to a miller trail blazer or bobcat 250. thanks
What does it have for a welding arc? The Trailblazers have a higher ac rectified frequency 3 phase welding arc. The Bobcats have single phase arcs. Wouldn't trade the Trailblazer arc for a lesser price single phase arc.
I love my trailblezer 280nt I do everything from stick-tig-wire-arc air- run the house when the power is out! and it welds better than any shop machine I have used. I love it!