- - By Junbao Zhang (*) Date 09-26-2007 06:06
hello,
  I have a PQR, it is dissimilar steel welding procedure. the joint position is 2G, carbon steel groove with buttering is lower, stainless steel is upper.
  I want to know if the PQR can fit to the condition, that is :  the joint position is 2G, carbon steel groove with buttering is upper, stainless steel is lower.
   thanks!
Parent - - By js55 (*****) Date 09-26-2007 13:36
Be a little more specific about the alloys. And unless there are some special circumstances not mentioned buttering for a ferritic/bainitic/martensitic to stainless steel is seldom required.
Parent - - By jon20013 (*****) Date 09-26-2007 14:04
Further, which Code?  If ASME IX, no problem unless as js55 states there are some unknown variables.  Reference QW-283 in the case of ASME IX.
Parent - - By Junbao Zhang (*) Date 09-27-2007 01:04
ASME IX,
Parent - - By jon20013 (*****) Date 09-27-2007 08:31
Position (or orientation in this case) is normally not an essential variable in these cases under ASME IX.
Parent - By Junbao Zhang (*) Date 09-27-2007 11:43
Thank a lot 
Parent - By js55 (*****) Date 09-27-2007 13:50
Nor should it be. ASME is right on this one. My 2 cents.