Since I have a PQR qualified with X60/X60 it means S1/S1, it can be used to support WPS for welding
X60/SA 350 LF2 it means S1/P1 ??
According QW 420.2 it should be OK.
It's my interpretation right ??
By
MBSims
Date
10-06-2007 15:56
Read this statement in QW-420.2:
"qualification using an S-Number
material qualifies corresponding S-Number materials but
not corresponding P-Number materials"
By
JCaprarulo
Date
10-17-2007 06:16
Thanks Marty, now it's clear.
Topic
Welding Industry
/
Technical Discussions
/ ASME IX Qualification S & P numbers.
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill