Weldah Welcome to the forum
Running vert up you should be at a 10 to 15 degree push angle. This would be slightly pointed up (pointed in the direction of your upward progression) rather than slightly pointing down as you are currently doing.
Your parameters are right on the money according to Lincolns own literature.. However they do note that stickout can be between 3/4 and 1 1/4 inches so you might find some benefit from extending your stickout a touch more.
http://content.lincolnelectric.com/pdfs/products/literature/c32000.pdfWith FCAW I prefer a slight side to side motion. (a wiggle rather than a weave) just to flatten the bead out. I would say that wiggle would be no wider than the wire diameter. Thats just how I like it.
Keep us posted on how it goes