Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Inspection & Qualification / Acceptance of ASNT level II
- - By dmilesdot (**) Date 10-12-2007 13:12
Are there other states besides New York and California that require an additional UT practical before allowing techs to perform UT?  Im not looking to open a can of worms here Im just curious of other states requirements.
Thanks
Dave
Parent - - By hogan (****) Date 10-12-2007 13:19
are you asking about dot work and/or structural?
Parent - By dmilesdot (**) Date 10-12-2007 13:28
hogan,
Structural or Bridge, D1.1 or D1.5 code work
Parent - - By CWI555 (*****) Date 10-12-2007 13:55
Those are the only two I am aware of currently. I've heard WA, OR, and Hawaii, but that is word of mouth, don't know for sure.
Parent - By hogan (****) Date 10-12-2007 14:02
some structural jobs will require fema 353. other than that there are no additional requirements for ut that i know of for OR and WA
Parent - - By g32141 (**) Date 10-13-2007 00:58
I do know for a fact that Virginia requires you to do a practical for RT (radiography) in order to do RT on their bridges.

I would guess that you would need the same to do UT if you didn't have an outside cert. I never asked nor had to take it though.

If you have an ASNT cert where you actually have test scores and did a practical (not grandfathered) would you still have to take the practical from the state of New York?
Parent - By dmilesdot (**) Date 10-15-2007 12:14
Anyone performing UT per the SCM must pass our practical.
Parent - By HgTX (***) Date 10-16-2007 19:47
Texas.
Up Topic Welding Industry / Inspection & Qualification / Acceptance of ASNT level II

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill