Dear Expert's,
While I am doing my procedure qualification test for 10" Pipe to Fittings, in that Pipe is in bottom and Fitting is in Top 6G position. After welding Magnetic particle test was conducted in that non relevent indication in the toe of weld was through out the joint.
Pipe Material: API X65
Fitting Material: ASTM F65
Why that indication appearing?
What metallurgical role playing?
Can I call it Magnetic writting?
Thanks
S.Senthilkumar