Thanks Lawrence. I think one of the problems that we have, Is that the only diameter wire that we can find is the .120 wire listed at cmw. Our supplier has it sanded or ground down to .065 for us , and I beleive it is contaminating the wire during this sanding process. We need to find it in the .062 diameter in a bright finish, or non sanded finish.