The Unit Cell (also called Bravais lattice) of ferrite is Body Centered Cube (BCC). That of austenite os Face Centered Cube (FCC).
On any book of Material Science (Callister, for example), you'll find figures illustrating how they look like.
Giovanni S. Crisi
Sao Paulo - Brazil