Chanadu,
I'm 100% with js55 when he says: "These alloys are used in such critical applications and are such crack sensitive alloys they should not be taken lightly."
The steel manufacturers should be the people to get in contact to, to pursue the correct procdures for welding their materials.
Just as a little hint from my side - as far as it's still unknown to you - here are two links treating the materials you are asking about.
First was an excellent article in the 08/2007 AWS Welding Journal and treating "P91 and Beyond":
http://files.aws.org/wj/2007/wj0807-29.pdf.Second leads to a paper coming from two German experts being with Böhler Thyssen and treating these materials as well:
http://www.msm.cam.ac.uk/phase-trans/2005/LINK/182.pdfHope this helps a bit.
Best regards,
Stephan
P.S. May God give Henry a quick recovery to enable him a quick return to the forums. I'm sure he would have tons of excellent information and personal experience on that.