Does ASTM spec SB-862-2 have a P number ?
Parent - - By dlmann (**) Date 11-07-2007 15:35
Hello Joe:
If your SB-862-2 is the same as SB-862 grade 2 then P No. 51.
Regards, Donnie Mann