- - By - Date 07-31-2000 13:35
I'm in the process of review a welding procedure for 5456 H116 alum base material, I have the tensile strenght base material, I can't locate the tensile strength for the filler material 5556. AWS 5.10 only give the chemical comp. Would ayone have this information? Thank you for your time.
Parent - By BP Maas (**) Date 08-01-2000 21:34
Average tensile strength 46,000 psi
Minimum annealed tensile strength 42,000 psi