I haven`t done d.h welding on pipe ,usually do small pipe installations on 6" sch.#40 pipe uphill and in position using stick 6011 and 7018 and would like to know if anyone could offer some tips,i.e. machine settings ,weave or no weave?,travel speed etc , thanks