Not logged in
American Welding Society Forum
Forum
AWS Website
Help
Search
Login
Topic
Welding Industry
/
General Welding Discussion
/ ***question***
By
52lincoln
Date
01-17-2008 00:40
what is the appendix C test
By
hogan
Date
01-17-2008 16:52
it is referenced in 6.12.5. it is an illustration of the RT acceptance criteria for tension welds. it is trying to show the acceptable amounts of different defects allowed by the code for that type of welded connection.
Topic
Welding Industry
/
General Welding Discussion
/ ***question***
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill