Not sure if this is the right part of the forum, but here goes.
My Miller 330 A/BP (mfd. 1984) works great, except for one thing - the post-flow timer wants to stick. I've heard these things are pretty pricey ($300+), and wondered if anyone had any insight as to how to get it going again. I thought I had the problem narrowed down to one IC (the 741 OP/AMP), but changing it didn't help. The rheostat and relay seem to ohm out OK, but I haven't been able to check any of the capacitors.
Is there a newer replacement for this unit, or has somebody been able to rig one together?