I would have to agree. About 10 years ago one of my clients built the same type header boxes that were about 15" X 20" X 1" thick. RT was required by the engineering folks, they would not allow UT. From what I recall not only film placement, but distortion and projection of the root area was a problem on the closure joint.
~thirdeye~