Ni Hard is a martensitic alloy composed by white cast iron and nickel, with a hardness of some 55 HRC. It's used for high abrasion resistance applications, such as ball mills lining. Bobfredtech is right, it's impossible to weld it. Sorry.
Giovanni S. Crisi
Sao Paulo - Brazil