- - By rafael Angarita (*) Date 02-04-2008 17:22
¿The LPT should be done before or after sandblasting?
¿Or first sandblasting, then welding and in the end LPT?
Parent - - By hogan (****) Date 02-04-2008 17:48
before
Parent - - By rafael Angarita (*) Date 02-04-2008 19:16
Can you be more explicit, please?
Parent - By Mikeqc1 (****) Date 02-04-2008 19:43
Certain cleaning operations are prohibited before Penetrant testing , as they could smear metal and close the indications you are looking for. These operations may include power wire brushing , grit blasting, and shot peening.
Sand blasting may be done to prepare for a weld( remove rust and Mill Scale) , then welded and the weld could be tested using the PT method, but sandblasting the weld would not be a good idea.
Parent - - By Lawrence (*****) Date 02-04-2008 19:57
Here is one example of instructions for liquid penetrant testing.

http://www.magnaflux.com/files/library/operating//Zyglo~reg_Kit_Operating_Instructions.pdf