I called this company and asked what the procedure is to get a job. I was expecting a 6" pipe test with either tig or 7018 root, but he told me that the procedure had changed. The test is 3 2 1/2" pipes all heavy wall in the 6G position with tig out with one, 7018 out on the other, and tig root and 7018 out on the other. Im thinking that is a hard test. Just was wondering what you all thought about this. O yea that is all 1/8 rods, gap, and land.