Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / General Welding Discussion / Miller Bobcat 250
- - By okwelder82 (***) Date 02-17-2008 22:09
Does anyone have a Miller Bobcat 250 that could tell me what setting they are useing to put an uphill 5p root in a 6 in piece of pipe. Ive only had the machine for a month or so and Im still trying to get the settings down. Now I know settings are for the most part a matter of personal preference but Im just looking for a place to start. Thanks.
Parent - By thewelder (***) Date 02-18-2008 04:16 Edited 02-18-2008 04:21
HI, I have a bobcat 225 and put my @ 85 amps, with 1/8 5p+, went the fit-up is 3/32 land and 3/32 root and on big pipe 90 to 95 amps on 1/8 land and 1/8 root, put the amps setting @ 70-150 and the fine ajustment work it betwing 3 and 4, i'll hope this help you.
Up Topic Welding Industry / General Welding Discussion / Miller Bobcat 250

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill