By CWI555
Date 02-21-2008 13:35
Edited 02-21-2008 14:42
ASME IX:07
QW-194 Visual Examination -- Performance
Performance test coupons shall show complete joint penetration
with complete fusion of weld metal and base metal.
Then you get into mechanicals or radiography whichever is the case.
QW-191.2.2 Acceptance Standards. Welder and
welding operator performance tests by radiography..etc..
Unless contract documents or other sections of the code stipulate additional criteria or reduction of criteria, it is as written in Section IX. Additions or reductions from the requirements of Section IX are not allowed otherwise.
Regards,
Gerald
As for penetration, there is no deminsion because it has to have complete penetration....all the way around. Therefor, if ANY portion does not have full penetration, no matter the length, depth, etc, it is rejectable.
As for undercut, as you know there is no criteria for it in sec IX. As far as I'm concerned, if there is no policy or if it's not written in the QC manual, you are only bound to what sec IX states. A lot of companies inspect the test coupon to the criteria for the code they are working to, but again, I would be careful if this is not spelled out somewhere in a company document.