Does any one know what/if the code requirement is for thermal couples when PWHT butt welds. example: can a shop "split" one lead 3 ways and then use one thermal couple on one weld to chart those 3 welds? If possible please reference code.I do know some client specs do not allow this type of set up, just wondering if there is a code restriction. Thanks!!