- - By ctrhenry Date 03-25-2008 14:43
Joint is a long slip fit .002 clearance, length is .75.

Joint will see operating temperatures of 800 f

Looking for a flux and a brazing rod/wire to use.

Thanks for any help
Parent - By Weldconsultant (*) Date 03-28-2008 06:25
Clearance and operating temperatures sound reasonable.  Best is to go through the HandyHarman guide to select the right flux/braze alloy combination for your application at the following link - there are options to braze in vacuum without use of fluxes (at high enough temperature, the surface oxides are reduced thus doing the same job as a flux).

http://www.handyharmancanada.com/TheBrazingBook/contents.htm#Index