By jrw159
Date 03-29-2008 02:30
Edited 03-29-2008 02:33
I have to agree with you on this. I have had more trouble in the past just getting engineering,they are busy, to put the neccessary information on the print, IE proper weld symbol, size, location, and God forbid if I need information on a groove weld that would require weld size, root opening, bevel %, finish contour and pertinant tail information. If they have the time AFTER the essential information is in place, then by all means use it. But is it manditory? I don't know.