Code: D1.2 (2003)
Application: Class II tubular structure
Material: 6061-T6 2x2x3/16" square tube
Process: GMAW, DCEN, ER4043, pure argon
We build a ton of these. One of our customers wants to perform in-process sample NDI and he's considering using eddy current. I'm not familiar enough with the process to understand how it will be used on this structure, which is about 80% fillets and the other 20% PJP grooves. My argument might be that this process will produce a lot of indications which are in the acceptable range of the code.