I am taking the 6g 2" pipe test with 6010 3/32 root 7018 3/32 caps. I am making landing of 3/32 with gap 3/32. Any option this set up?
The test lets make your own landing, set your own gap. Which is the usual total v groove 60 or 70 degree for the test?