The properties of the 6061 would be predicable after heat treat, but with the 4043 filler, the strength of the weld will depend on how much dilution took place since the weld would be relying on any precipitation strengthening from elements picked up from the base metal. Typically a 4043 weld is not considered heat-treatable.