What's the opinion on this?
A Purchase order calls for a material SA-234 wpb 8" SCH 40 Butt weld cap purchased under ASME boiler and pressure vessel code section VIII DIV 1 usage.
Now here is the situation I have received a Certificate of Compliance for this material (along with others on the same C of C) I looked at my code book for SA-234 WPB the spec calls out CAR, MAN,PHOS,SUL,SI,CHR,MOLY,NIC,CU,VAN.
The C of C has all Chems except MOLY and VAN (no value for these two chems).
I have questioned this and asked that these be given some value on the report (for all I know they were left out unintentionally. What I was given back in response was a copy of an ASTM spec (Date issue unknown) and a note stating that there is no requirement for those Chems (although there are other reported Chems that have no requirements on the C of C).
ASME states other acceptable astm specs 82a thru 04
My copy of ASTM -02 is identical to my ASME -04 (except ASTM gives a max on COLUMBIUM) both give max values for VAN, and MOLY.
I have been told that a blank should be taken as 0.0000% or it need not be reported. The unknown issue of ASTM implies that there are no requirements for those chems.
Any opinion would be helpful on how I can resolve this, or steps can take to get to the bottom it.
Not quite sure if this is an issue or I just can't see the forest though the trees.
if any1 needs more info or a better expination please ask.