Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / General Welding Discussion / rig welder pay for ND
- - By stanantonio Date 04-24-2008 07:08
[deleted]
Parent - - By snuffman (***) Date 04-26-2008 02:30
[deleted]
Parent - By Cactusthewelder (*****) Date 04-26-2008 13:03
I worked in ND in 05. The rate was 80.00 pr hr then. I am sure it is higher now with the cst of fuel.
Parent - By stanantonio Date 05-02-2008 04:59
Most people around here are still charging the same rate there snuffman.
Parent - - By ndlssrd Date 04-28-2008 00:34
Over hear in Montana we are getting somewhere around 75-85 per hour.  Includes everything.  Where are you in N.D.?
Parent - By stanantonio Date 05-02-2008 05:02
Thats a pretty good deal there. Do you have to have an Umbrella pollicy?  I been working in the williston area mostly a little in Sidney Mt
Parent - - By BadgerWelds (*) Date 04-29-2008 01:48
Here in Central SD we are getting $85.oo/ Hr every thing included.. There are some cut raters around here doing it for half price,but doing a halfrate job.
Parent - By ZCat (***) Date 04-29-2008 02:17
How many hours are all you guys having to work?
Parent - - By stanantonio Date 05-02-2008 05:09
thats pretty good there badgerwelds.  what are you doing in SD pipline?
Parent - - By BadgerWelds (*) Date 05-03-2008 02:11
Yes Stanantonio it is pipeline stuff..
Parent - By stanantonio Date 05-07-2008 04:15
thanks for the info what you told me means I should pretty much raise my rates.  Company's are sometimes weird.  they seem to always look for bottom dollar yet they dont that bottom dollar dosent always mean the cheapest.( In terms of weld inches, consumables, equipment, ect.)
Parent - - By leterburn (**) Date 05-13-2008 01:55
Stanantonio - Been getting 80 / hr and 100 / day here...  but haven't been hooked up as much as I'd like...  any work further West in ND????  Been in between Minot / New Town.
Parent - - By stanantonio Date 05-13-2008 05:10
yeah there is plenty of work here in the west  What have you been mostly working on?
Parent - - By leterburn (**) Date 05-13-2008 15:54 Edited 05-13-2008 16:10
pipelines mostly - would sure like a larger run ( stuff I've been on anywhere from 3-7 miles - 4"-12" so far) or some steadier work - also recently qualified for Enbridge on sleeving, branch, 6G up/down - but not OQ'd yet / work not starting until later in the month.
Parent - - By stanantonio Date 05-14-2008 02:03
yeha same thing here The lines seem to be pretty short.  What insurance requirements does enbridge want. Never really tried to pursue them.
Parent - By leterburn (**) Date 05-15-2008 03:29
I carry 2 million...  but working under a good friend of mine on that tank tie-in.  I believe he has 1 million umbrella to boot after the 2 mil.
Up Topic Welding Industry / General Welding Discussion / rig welder pay for ND