as far as you mean the full austenitic heat resistant filler wire having a composition as follows:
- C: .12%
- Si: .30%
- Mn: 4.5%
- Cr: 2.1%
- Ni: 33%
- Nb: 1.2%
- Fe: Remainder
we do have a specific standard "Material Number" (Werkstoffnummer) in Germany which is ~ 1.4850 (X15NiCrNb32-21).
This number again is comparable with your ASTM: A 167.
As far as I have seen it appears that no AWS designation exists yet, but please see also the attached pdf.