- - By Windrider Date 05-21-2008 14:17
[deleted]
Parent - - By jrw159 (*****) Date 05-21-2008 14:52
Windrider,
  You have not mentioned what, if any, code. Looking in AWS D1.1 for "groove welds" since I could not find referance to "butt welds" only "butt joints" I see 2.3.1.2 Effective size of CJP groove welds. Maybe this referance will help.

jrw
Parent - By Windrider Date 05-21-2008 15:17
sorry for the term being wrong, I meant butt joint.
Tom