During GTAW.......what is meant by "cold wire feed",,,,,"hot wire feed"......?
By
Lawrence
Date
05-22-2007 11:23
Here is an explaination from Jetline
http://www.jetline.com/HWP-50D%20Brochure.pdf
In "Hot Wire" GTAW current is run through the filler, the resistance heats it and the result is increased deposition... I think it us usually a semi-auto or mechanized GTA process.
"Cold Wire" is plain ol hand feed of bare rod.
By
JA
Date
05-22-2007 12:57
Thank you Lawrence.......
Topic
Welding Industry
/
Technical Discussions
/ cold & hot wire feed....
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill