one4fatman, what do you need to know about A106? It is an ASME P-Number 1 material and readily weldable with 70 series filler. At the thickness you're using you may need PWHT depending on Code of Construction. If you need specific detail define exactly what you're looking for and send me an e-mail so I can send you additional information.