By
Weldway
Date
06-22-2007 14:34
When doing a t weld fillet with 1/8th in. plate is the qualification good for any thickness less than 1/8th and up to 1/4 in.?
By
pax23
Date
06-22-2007 19:27
If this is a D1.1 question, then this is covered by Table 4.4. Table 4.4 tells us the max is unlimited and the minimum is 1/8" (see note a).
Topic
American Welding Society Services
/
Technical Standards & Publications
/ D1.1 WPS Qualification size range fillet
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill